Foshan Steel refers to the structure mainly composed of steel materials, is one of the main types of building structures. Structure is mainly made of steel and steel plate, such as steel beams, steel columns, steel trusses and other components, the components or components are usually used between the weld, bolt or rivet connection. Because of its light weight, and the construction is simple, widely used in large factories, venues, high-level and other fields.
Steel structure in the welding process, there are many matters needing attention, once negligent, there may be a big mistake.

1. Welding construction does not pay attention to choose the best voltage
【phenomenon】
Welding, whether it is rendering, filling, cover, regardless of groove size, are selected the same arc voltage. This may not meet the requirements of the penetration, melting wide, undercuts, stomatal, splash and other defects.
【Measures】
Generally should be selected for different situations corresponding to the long arc or short arc to get a better welding quality and efficiency. For example, primer welding in order to be able to get a better penetration of short arc operation should be used, filled with welding or cover surface welding in order to get higher efficiency and melting width can be appropriately increased arc voltage.

2. Welding does not control the welding current
【phenomenon】
Welding, in order to grab the progress of the butt weld for the plate to take not open groove. Strength index decreased, or even less than the standard requirements, bending test cracks, so that the weld joint performance can not be guaranteed, constitute a potential hazard to structural safety.
【Measures】
Welding process according to the assessment of the welding current control, allowing 10 to 15% floating. Beveled edge of the groove size should not exceed 6mm. Butt joint, the thickness of more than 6mm, to open the groove for welding.

3. Do not pay attention to welding speed and welding current, electrode diameter in coordination.
【phenomenon】
Welding does not pay attention to control the welding speed and welding current, electrode diameter, welding position coordination to use. Such as the full penetration of the angle seam backing welding, due to the root size is narrow, such as welding speed too fast, the root gas, slag does not have enough time to discharge, easy to root imperfect penetration, slag, porosity and other defects ; Cover surface welding, such as welding speed too fast, but also easy to produce pores; welding speed is too slow, the weld residual height will be too high, irregular shape; welded sheet or blunt edge size of the small weld, the welding speed too Slow, prone to burn through and so on.
【Measures】
Welding speed, welding quality and welding production efficiency have a significant impact, when used with the welding current, weld location (bottoming, filling welding, cover welding), the thickness of the weld, groove size selection of the appropriate welding speed, To ensure penetration, gas, welding slag easy to discharge, do not burn through, under the premise of forming a good selection of larger welding speed, in order to improve productivity efficiency.

4. Do not pay attention to control arc welding length
【phenomenon】
Welding is not based on the groove form, the number of welding layers, welding forms, electrode type and so appropriate to adjust the length of the arc. Due to improper use of welding arc length, it is difficult to obtain high quality weld.
【Measures】
In order to ensure the quality of the weld, welding generally use short-arc operation, but according to different situations to choose the appropriate arc length to obtain the best welding quality, such as V-shaped groove docking, corner of the first layer should be used Short arc to ensure penetration, and does not happen undercurrent phenomenon, the second layer can be slightly longer to fill the weld. Weld gap time is appropriate to use short arc, the arc can be a little longer when the arc, welding speed. Up welding arc should be the shortest to prevent molten iron downstream; vertical welding, horizontal welding in order to control the bath temperature, but also with small current, short arc welding. In addition, no matter what welding, in the course of the movement should pay attention to always keep the arc length is basically the same, in order to ensure that the entire weld melting width and penetration consistent.

5. Welding does not pay attention to control welding deformation
【phenomenon】
Welding not pay attention to the welding sequence, staffing, groove form, selection of welding methods and methods of operation and other aspects of control deformation, resulting in large deformation after welding, correction difficulties, increase costs, especially heavy plate and large parts, the correction is difficult , With mechanical correction can cause cracks or lamellar tear. Flame correction with high cost and poor operation easily lead to overheating of the workpiece. For the workpiece with high precision, it does not take effective control deformation measures, will lead to the workpiece installation size can not meet the requirements, or even cause rework or scrap.
【Measures】
The use of reasonable welding sequence and use the appropriate welding specifications and methods of operation, but also the use of anti-deformation and rigid fixation measures.

Copyright:佛山市勝邦鋼結構有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粵ICP備13078463號
主站蜘蛛池模板: 天下机械|机床商讯-机械网|机械技术|机械信息|机床资讯|机床设备|机床商讯杂志 | 久久黄色一级视频_视频一区精品自拍_理论片免费ā片在线观看_亚洲色视频在线播放网站_香港经典a毛片免费观看_亚州三级久久电影 | 和远智能-和远智能科技股份有限公司| 找刑事辩护律师_找深圳刑事律师多少钱★王平聚【清华博士/刑法教授】 | 宁波明驰同步带有限公司| 清洁公司| 保洁公司| 东莞清洁| 东莞保洁|壹壹清洁 | 频谱矢量网络分析仪_鼎阳数字示波器-苏州东伟元电子有限公司 | 上海希喆机械有限公司-Schunk雄克,雄克卡盘, 雄克机械手, B+R贝加莱, ELCIS编码器,艾西斯编码器, TWK编码器,Nexen,Joyce dayton升降机,Thomson汤姆森,TPG减速机,INA导轨。 | 明康食品有限公司 -方集馓子 亨特小麻花 | 真空热处理-渗碳热处理-氮化热处理-[东莞德亿]专业热处理加工厂家 | 以物联网技术为核心专注于智能安防领域物联网服务的高新技术企业-北京欣智恒科技股份有限公司(官网) | 金坛区成辉仪器厂-精密増力电动搅拌器,石英亚沸蒸馏水器- | 双合金螺杆|注塑机螺杆|挤出机螺杆|双合金料管—东莞市精耐螺杆机械有限公司 | 制沙机,反击式破碎机,重锤破碎机,泥石分离机,圆锥破碎机厂家-昆明德鑫机械 | 亿企商贸-亿万企业的商务贸易平台-B2B企业产品发布供求信息平台,一带一路中国企业及产品展示平台,免费企业智能自助建站网络营销推广平台,打造B2B企业黄页产品信息发布推广专业综合电子商务平台! | 孝感东方妇科医院_孝感妇科医院哪家好_孝感人流多少钱 | 卫生间隔断-东莞卫生间隔断-东莞卫生间隔断厂家-公共卫生间隔断-东莞市康丰家居建材有限公司 | 戏曲下载网,唱戏机戏曲下载,戏曲视频下载,戏曲MP3下载 - 梨园风 | 太原门禁系统_太原车牌识别_山西人脸识别系统-山西元一智能科技有限公司 | 智能灰熔融性测试仪,微机自动定硫仪,快速自动测硫仪-鹤壁市恒科仪器仪表有限公司 | 永州市冷水滩华立水力机械设备有限公司| 诸城市佳品食品机械有限公司| 南宁清洁公司|外墙清洗|开荒清洁|洒水车|管道疏通|园林绿化_广西优而美环境工程有限公司 | 钱眼网-透过钱眼看商机| 太原石膏基自流平,太原轻质抹灰石膏,太原腻子粉,太原抗裂砂浆-太原乔贝建筑材料有限公司 | 妙手网-圆心大药房-广东圆心恒金堂医药连锁有限公司-放心的网上药店_妙手医生旗下正规网上买药平台 | 九江守信建筑工程有限公司| 深圳起重机,龙门吊,天车起重工程,电动葫芦,液压升降货梯-深圳市德力起重机械有限公司 | 兰州职业学校-新华互联网学校咨询平台中心 | 威学一百-专注国际学校择校备考-DSE-A-level-雅思-托福-OSSD-港澳台联考-AP-IGCSE-IB-AMC-多邻国-PTE-SAT-SSAT-小语种(如日语,韩语,德语,法语,西班牙语,意大利语,俄语,泰语)等考试培训,为出国留学学生提供个性化定制性学习方案,线下实体面授+线上网络课程, 提供一对一,小班课等多种班型 | 全自动滤水器_射水抽气器_气液两相流疏水器-连云港神美电力辅机有限公司 | 实木运动地板价格_运动木地板厂家-欧氏实木运动地板网 | 新一能-配电箱、变频柜、plc控制柜、开关柜生产厂家 | 太阳能路灯 太阳能路灯厂家 路灯厂家-保定正联光电科技有限公司 太阳能光伏发电_太阳能热水器_空气能热水器_直饮净水器_深圳市大兴节能环保科技有限公司 | 西安真石漆_无机涂料厂家_无机涂料多少钱一个平方—陕西秦森环保科技有限公司 | 球形钢支座,粘滞阻尼器,抗震球型钢支座,盆式橡胶支座,调谐质量阻尼器,屈曲约束支撑-衡水路泽科技 | 钻机配件-岩心管-岩心管接箍-地质套管-煤矿用钻头-河南滨远机械设备有限公司 | 山东万利精密机械制造有限公司-高速金属圆锯机,数控高速圆锯机,高速圆锯机生产厂家 | 江阴月子会所-江阴月子中心-江阴坐月子、月子护理哪家好-乐茵月子中心 | 找网页游戏鬼服 高返利鬼服游戏平台 鬼服开服表 - 猫游戏鬼服大全 | 免费会员管理系统,会员管理软件,会员卡积分系统—智络软件 |